Browse & Explore

Search & Select

A517(A) (High strain steel grade)

Description

General

(Ferro (Fe) rest, cupper (C) 0.15-0.21, Silicon (Si) 0.40-0.80, Manganese (Mn) 0.80-1.10, Chromium (Cr) 0.40-0.80, Molybdenum (Mo) 0.28, Zirconium (Zr) 0.05 (wt.%))

Properties

Chemical properties

Minimum value Maximum value Unit Sources
%
%

Electrical properties

Minimum value Maximum value Unit Sources
kV/mm
%
-0.45 -0.45 V
Ohm.mm²/m

Manufacturing Properties

Minimum value Maximum value Unit Sources

Mechanical properties

Minimum value Maximum value Unit Sources
MPa
MPa
MPa
7850 7850 kg/m³
18 18 %
MPa
0.25 0.3 J/cm
MPa
790 790 MPa
MPa
690 690 MPa
205000 205000 MPa

Optical properties

Minimum value Maximum value Unit Sources

Thermal properties

Minimum value Maximum value Unit Sources
°C
1500 1540 °C
°C
J/kg.K
W/m.K
13 13 e-6/K

Environment

4.39 mPt
0.09 Pt
9820 mELU
3.65 MJ/MJ
23.3 MJ
3.15 kg
0.01 kg
Environmental data for the production of 1 kg crude steel from SPIN. Transport is added. The coal comes for 65% from Canada, 23% Australia, 12% from the EEC. Iron ore comes for 37% from Brasil, 21% Australia, 31% Europe and the remaining 11% from elsewhere. Lime is imported from Belgium. The production and emission data are for 1989.
Idemat 2003, Design for Sustainability, Delft University of Technology