| Quantity | Value | Unit |
| Young's modulus | 41400 - 44800 | MPa |
| Tensile strength | 19 - 19 | MPa |
| Yield strength | 9 - 9 | MPa |
| Quantity | Value | Unit |
| Thermal expansion | 35 - 35 | e-6/K |
| Melting temperature | 228 - 228 | °C |
| Density | 5750 - 5750 | kg/m3 |
| Resistivity | 0.115 - 0.115 | Ohm.mm2/m |
| Electrochemical potential | -0.14 - 0.151 | V |
| Quantity | Value | Unit |
| Eco indicator 95 | 12 | mPt |
| EPS | 1510000 | mELU |
| Ex (in) / Ex (out) | 54.4662309368192 | MJ/MJ |
| GER | 228 | MJ |
| Raw materials input | 6.6081046534271 | kg |
| Solid | 0.1027337 | kg |
| Eco indicator 99 | 15.3 | Pt |
| Environmental remarks | Tin is mainly found as SnO2 (cassirite) with a metal percentage of 55%. Important producers are: Brasil 23%, Malasia 14%, Indonesia 14% and China with 12%. Often (87%) in open mining. The amount of recycling is 8.7% | |
| Remarks | Tin is extremely hazardous and use should be prevented. | |
Sample: Other Metals |
||
![]() |
Dear visitor, Matbase has not changed a lot over the last few years, but, as you may have noticed, read more
Richard Vennix MSc
co-founder of Matbase and innovation consultant
08-12-2009 08:33
Last november was a memorable month for us at Matbase, we passed the milestone of 1000 visitors per day. So I guess we were not that far of when we thought it would be a good idea to make the material database we used as students during our stay at the Delft University of Technology accessable to other people. Apparently, people appreciate the easy way they can lookup the material properties and how we present the data.
Read more »