Data Table for: Non-ferrous Metals: Cast Copper: G-CuSn12

Mechanical Properties

Quantity Value Unit
Young's modulus 105000 - 105000 MPa
Shear modulus 39000 - 39000 MPa
Tensile strength 260 - 260 MPa
Elongation 12 - 12 %
Yield strength 140 - 140 MPa

Physical Properties

Quantity Value Unit
Thermal expansion 18 - 18 e-6/K
Specific heat 380 - 380 J/kg.K
Melting temperature 820 - 990 °C
Density 8600 - 8600 kg/m3
Resistivity 0.15 - 0.15 Ohm.mm2/m

Environmental Data

Quantity Value Unit
Eco indicator 95 88.5 mPt
EPS 244000 mELU
Ex (in) / Ex (out) 58.3333333333333 MJ/MJ
GER 111 MJ
Raw materials input 3.86841451545286 kg
Solid 117.91390069 kg
Eco indicator 99 4.06 Pt
Environmental remarks Considerable differences appear in practice. Therefore we used the energy requirements of winning in open mines and melting in the main producing countries US and Chile as basis. The sulfidic ore has a copper content of 0,6%. There is also a wide spread in the emission of SO2 during the refinery process. This reaches from 38 gram/kg Cu to 3500 gram/kg Cu, with an average of 1060gram / kg Cu. Often the reclaimed SO2 is used for the production of sulphuric acid. The world avererage scrap percentage is 20%.

General

     
Remarks (Cu rest, Sn 12 (wt.%))

Sample: Cast Copper