G-CuSn 10

Category Type Material
Non-ferrous Metals Cast Copper

show all types of Non-ferrous Metals

G-CuAl10Fe
G-CuAl10Ni
G-CuNi10
G-CuSn 10
G-CuSn12
G-CuSn5Zn5Pb5
G-CuZn 40
G-CuZn15
G-CuZn37Pb

Data Table for: Non-ferrous Metals: Cast Copper: G-CuSn 10

Mechanical Properties

Quantity Value Unit
Young's modulus 100000 - 100000 MPa
Shear modulus 37000 - 37000 MPa
Tensile strength 270 - 270 MPa
Elongation 18 - 18 %
Yield strength 130 - 130 MPa

Physical Properties

Quantity Value Unit
Thermal expansion 18 - 18 e-6/K
Thermal conductivity 67 - 67 W/m.K
Specific heat 380 - 380 J/kg.K
Melting temperature 845 - 1010 °C
Density 8700 - 8700 kg/m3
Resistivity 0.13 - 0.13 Ohm.mm2/m

Environmental Data

Quantity Value Unit
Eco indicator 95 90.21 mPt
EPS 215000 mELU
Ex (in) / Ex (out) 58.6734693877551 MJ/MJ
GER 108 MJ
Raw materials input 3.80549007471106 kg
Solid 120.61187935 kg
Eco indicator 99 3.61 Pt
Environmental remarks Considerable differences appear in practice. Therefore we used the energy requirements of winning in open mines and smelting in the main producing countries US and Chile as basis. The sulfidic ore has a copper content of 0,6%. There is also a wide spread in the emission of SO2 during the refinery process. This reaches from 38 gram/kg Cu to 3500 gram/kg Cu, with an average of 1060gram / kg Cu. Often the reclaimed SO2 is used for the production of sulphuric acid. The world avererage scrap percentage is 20%.

General

     
Remarks (Cu rest, Sn 10.0 (wt.%))